Contribution of Compounding and Mixing in Cost Reduction of Pvc Products
Introduction:
One of the nine ways to reduce cost in PVC processing industry is to reduce cost of the compound.
Compounding and mixing are the two sub processes for the preparation of dry blend for further processing; be it extrusion, injection moulding etc.
First step is to understand the product requirements, not only in terms of the dimensional, mechanical, thermal or electrical properties, but mainly under which environmental conditions the product has to perform. This is because to make customer happy, the product must perform as per customer expectations and not alone as per product requirements (total requirements).
Having understood performance requirements for PVC products, the next step is to “design a compound” to meet these total requirements.
Compounding process deals with deciding – Which additives to add (selection of stabilizer, lubricant, plasticizer, process aids, impact modifiers, filler etc.), Why to add (to achieve smooth processing with optimum fusion, properties and performance requirements) and How much to add (recipe).
The next step would be to mix these additives and PVC homogeneously; to get a dry blend ready for further processing. Mixing is not a simple blending of the ingredients; rather it is a complex process.
Mixing process deals with –When to add (mixer speed, sequence, temperature), Where to add (hot mixer or cooler mixer), How to add (in the beginning, at specific temperature or towards the end) and What to control (Dispersion, Distribution, Diffusion to homogenize –DDD).
Batch to batch variation should be minimized by achieving consistency between the batches in terms of Time-Temperature-Torque (TTT) during mixing. Continuous mixing process is desirable in case of mass production. Producing consistent compound that assures product’s desired performance at minimum cost has to be the focus of the process owner. This is indeed the purpose of quality assurance.
Dry blend has to be free flowing at 40-45 °C and have consistent bulk density for conveying and smooth processing.
Production cost consideration for compound:
90% problems related to processing, quality and performance find its root in the compound.
Formulations need to be tailor made. A copy paste formulation from other industry or a book may not work at all in terms of smooth processing or properties of product; leave apart the performance of the product, even if costly ingredients are used. This ultimately increases cost of production.
Most of the processors wrongly think that mixing is merely a blending process, hence they use casual workers in compounding and mixing and to tackle almost irreversible problems originated from this, they employ highly paid managers, mostly from engineering background rather than technology background. Also, periodic maintenance of mixers is neglected under the pretext of non stop feeding requirement of compound to production so that the line does not break. Imagine what could happen if these casual workers are used for weighing the additives! Being casual, their approach for weighing will also be casual. Everyone is aware of what could happen due to weight variation in additives and its cascading effect on costs.
Compounding and mixing requires a separate process owner:
Many organizations consider compounding and mixing process as a part of extrusion/moulding process, under same process owner who hardly visits mixing department. This is usually done at small industry level. But for medium/large scale industries, it is advisable to have a separate process owner for mixing section, who does justice to the process and also visit his immediate customer, the production area, to find areas for improvement in compounding.
Cost should be considered in totality:
Many processors only focus on cost reduction of the compound. If compound cost is increased, it becomes a big bothering point for them. They don’t consider whether the OEE for extrusion or moulding is excellent. This is a wrong approach.
Consider a case where cost of the compound is increased by Rs. 1/Kg by replacing certain additives to improve processability, and as a result cost of production is reduced by Rs. 4/Kg. The net cost reduction would be Rs.3/Kg. It shows that the costs must be considered in totality and not for compound only.
Most popular way of reducing the cost:
Most of the people look at cost reduction in terms of adding more filler. They believe that by adding cheaper filler of almost twice the specific gravity of PVC, the cost would reduce substantially. There are several articles published to highlight the fact that deciding the cost of compound is not in terms of Rs/Kg, but the realistic way is to calculate cost in terms of Lit /Kg.
Since for the same dimensions of pipe with higher CaCO3 content, the weight of the pipe or profile increases, on e must understand that it is the additional compound and not the filler that goes into the pipe or profile. Many processors cleverly reduce the weight of the pipe to compensate. This reduces the thickness as well as the quality. The wear and tear of screw and barrel is not considered by such processors. This wear and tear in the screw and barrel actually reduces the flow over a period of time, increases the residence time of compound in the extruder and the compound demands more stabilizer that eventually increases the cost. Is it cost cutting or cost reduction?
CaCO3 does not melt during processing, hence with increase in CaCO3, the melt viscosity increases. Therefore flow rate decreases and number of pipes per hour reduces even after adjusting the lubrication, but Kg/Hr is more. Since pipes are sold per metre basis, to what extent this would help?
However, if product justifies use of higher level of CaCO3, there is no harm in using it subject to the acceptance by respective standards. For example SWR pipes use 20-25 Phr, while floor tiles use 100-150 Phr filler. Also, varieties of grades of CaCO3 are available – ground, precipitated and coated, in various particle sizes and so on.
Judicious use of additives in the compound can reduce the cost:
Stabilizers, lubricants, plasticizers are seldom added at individual level; they are always added as stabilizer system, lubricant system and plasticizer system etc, consisting of synergistic components.
Multi-functional additives are preferred. There is nothing wrong in using one pack additive, but one must understand that one pack systems are like readymade garments as against tailor made garments, sometimes one has to suitably modify it by adding extra additives based on screw/barrel condition, extrusion speed, diameter of pipe/profile; filler content etc, if one wants best quality.
Cost reduction through testing of raw materials:
Most of the processors use same formulations even if the raw materials and additives are of inconsistent in quality. Extruder operator has to struggle with the processing parameters to tackle the inconsistency in the formulation. In such trial and error cases the product is not consistent and wastage is more.
Those who understand this aspect test the raw materials and modify formulations accordingly. Use of torque rheometer to match the graph with successfully running formulation is the best way. The advantage is that the operator need not change the parameters and achieves consistent production with minimal wastage. This reduces the cost in totality.
Thus, instead of keeping the same formulation and changing the process parameters, it is advisable to modify the compound and process it at same parameters. The operator uses the free time to look after other important aspects like Jishu Hozen. This approach reduces the cost.
Share this article: